Service Temperature: | -200°C To 650°C | Melting Point: | 1000-1200°C |
---|---|---|---|
Density: | 60-100 Kg/m3 | Tensile Strength: | ≥7 KPa |
Moisture Resistance: | Non-hydrophilic | Environmental Impact: | Low |
Fire Resistance: | Class A | Thermal Conductivity: | 0.035-0.044 W/mK |
Sound Absorption: | 0.75-1.05 | Incombustibillty: | A |
Acidity Coefficient: | 1.6 | Chemical Resistance: | Resistant To Most Acids And Alkalis |
Material: | Mineral Wool | Compression Strength: | ≥40 KPa |
Highlight: | Walls Rockwool Insulation Blanket,Rock Wool Wired Blankets Used,Large Pipe Rock Wool Blanket |
Technical Data | ||
Properties | Blanket | Standards |
Density Tolerance | ±10% | GB/T 19686-2005 |
Fire Performance
|
Non-Combustible | GB/T 5464-1999 |
Reaction to fire Class A1 | GB/T 8624-2006 | |
Thermal Conductivity(W/mK,at70±5℃) | ≤0.044 | GB/T 10295 |
Fiber Diameter | 7(+/-1)um | GB/T 5480. 4 |
Shot Content(shot size>0.25mm) | ≤12% | - |
Moisture Content | ≤0.5% | - |
Organic Matter Content | ≤4% | - |
Melting Point | >1000℃ | - |
Main application:
Advantage:
Specification:
Product | Blanket |
Density (kg/m3) | 60-100 |
Size :L x W (mm) | 600X5000 |
Thickness (mm) | 30-150 |
Product introduction of the stone wool Blanket
FANRYN Stone wool blanket is made from natural rocks such as basalt and limestone. The rocks are melted in
a cupola at temperature of >1450 ℃, and the molten lava is fiberized by a spinner. The inorganic fibers are bonded
together using a thermosetting resin to form the final product which is cut into suitable sizes for easy handling and
installation.
STONE WOOL blanket is widely used in public, commercial and residential buildings as well as industrial plants,
for applications such as roofing, external wall, partition wall and floating floor to provide fire protection, thermal insulation,
acoustic control and condensation control.